The Ultimate Guide To aluminium extrusion
The following factor is to cut the cylindrical billet from a stretched log of material, then preheat the billet within an oven to 400-500ᵒC. This technique prepares the billet, making it malleable for the operation. It ensures that it is not molten.Changing the design on the aluminum extrusion cross-portion, setting good tolerances, and choosing